Stainless steel bar trade flows: who imports from where (HS 7222), EU 2025 and US 2024
November 21, 2026
The EU27 imported 846.8 million euros of stainless steel bars, rods and sections (HS 7222) from outside the bloc in 2025, and India supplied 57 percent of that value and 78 percent of the tonnes. The United States imported 770.0 million dollars of the same goods in 2024, and Italy led with a third of the value. This post gives the tables, says which statistics each one comes from and shows where two sources disagree.
We give no trade advice. Figures were read on 25 October 2026. The Eurostat data were last updated on 16 October 2026, and 2026 months are provisional.
What the code covers
HS 7222 is the stainless bar a turning shop buys. Its five six-digit lines split into hot-rolled round bar, other hot-rolled bar, cold-formed or cold-finished bar, other bar and rods, and angles, shapes and sections. Stainless wire (7223) and hot-rolled bar in irregularly wound coils (7221) are separate. Machined parts are classified under the heading for the finished article, as our guide to the Section 232 duty on stainless parts shows, so this is stock and not parts. The same tariff block carries the heaviest duty in that guide, which is one reason origin matters.
EU27: imports from outside the bloc
Eurostat’s Comext database reports the EU27 as one reporter. Its extra-EU imports of HS 7222:
| Year | Value, million euros | Tonnes | Unit value, euros per kg |
|---|---|---|---|
| 2023 | 943.9 | 208,939 | 4.52 |
| 2024 | 835.0 | 207,118 | 4.03 |
| 2025 | 846.8 | 245,018 | 3.46 |
| January to August 2025 | 632.7 | 176,995 | 3.57 |
| January to August 2026 (provisional) | 512.0 | 152,165 | 3.36 |
The unit values are our arithmetic, value divided by weight. Value in January to August 2026 is 19 percent below the same months of 2025 and tonnes are 14 percent below. Monthly imports arrive in large lumps: value was about 147 to 179 million euros in the first month of most quarters (January, April, July and October 2025) and 18 to 32 million in the other months. We do not know the cause. The EU steel import regime sets quota volumes by quarter, which would fit, but the statistics cannot confirm it.
Origins, 2025
| Origin | 2024, million euros | 2025, million euros | Share of 2025 value | 2025 tonnes | 2025 euros per kg |
|---|---|---|---|---|---|
| India | 443.2 | 481.8 | 57% | 190,847 | 2.52 |
| United Kingdom | 100.2 | 96.5 | 11% | 10,994 | 8.78 |
| Switzerland | 94.6 | 78.4 | 9% | 14,137 | 5.55 |
| United States | 77.3 | 72.6 | 9% | 2,746 | 26.44 |
| Taiwan | 36.6 | 37.2 | 4% | 8,162 | 4.56 |
| China | 31.5 | 31.8 | 4% | 11,405 | 2.79 |
| All other origins | 51.6 | 48.5 | 6% | 6,727 | 7.21 |
| Extra-EU total | 835.0 | 846.8 | 100% | 245,018 | 3.46 |
India’s share was 57 percent in 2023, 53 percent in 2024 and 57 percent in 2025. By tonnes it is much larger, and its low unit value points to a different product mix from the UK, Swiss and US lines, which are small tonnages at high values. The statistics do not show grades or sizes, so we cannot say what each supplier ships.
By product line, 2025
| Line | Value, million euros | Tonnes |
|---|---|---|
| 722220 cold-formed or cold-finished bar | 451.3 | 132,828 |
| 722211 hot-rolled round bar | 132.1 | 37,013 |
| 722230 other bar and rods | 119.1 | 29,467 |
| 722240 angles, shapes and sections | 100.7 | 30,223 |
| 722219 other hot-rolled bar | 43.5 | 15,488 |
Cold-finished bar, the form many turned parts start from, is 53 percent of extra-EU value.
Most EU supply is inside the EU
For the EU27, Comext reports 2,126.7 million euros and 508,470 tonnes of HS 7222 moving between member states in 2025. Adding the extra-EU 846.8 million, about 72 percent of the bar the bloc received by value came from within it. EU mills also export: extra-EU exports were 1,189.9 million euros in 2025, down from 1,417.2 million in 2024 and 1,543.6 million in 2023. The United States took 345.2 million euros of that in 2025, down 24 percent from 451.6 million in 2024.
United States: imports in 2024
The latest US figures we could read are for 2024, from CEPII’s BACI database. The UN Comtrade preview service was out of quota while we worked, and the USITC DataWeb needs a login that we did not use, so check 2025 there. BACI reconciles the importer’s and exporter’s reports and puts imports on a free-on-board basis, so its values differ from US customs figures.
| Origin | Value, million US dollars | Share | Tonnes | Dollars per kg |
|---|---|---|---|---|
| Italy | 250.5 | 32.5% | 40,019 | 6.26 |
| Germany | 96.3 | 12.5% | 15,972 | 6.03 |
| Taiwan | 94.8 | 12.3% | 18,540 | 5.11 |
| India | 86.9 | 11.3% | 21,149 | 4.11 |
| Portugal | 52.8 | 6.9% | 9,763 | 5.41 |
| Ukraine | 27.2 | 3.5% | 5,623 | 4.83 |
| Spain | 19.2 | 2.5% | 3,941 | 4.88 |
| United Arab Emirates | 18.2 | 2.4% | 6,116 | 2.98 |
| All other origins (61 countries) | 124.0 | 16.1% | 18,392 | 6.74 |
| Total | 770.0 | 100% | 139,515 | 5.52 |
EU members together supplied 479.3 million dollars, 62 percent of the total. US imports were 580.0 million dollars in 2021, 841.8 in 2022, 863.4 in 2023 and 770.0 in 2024. Italy’s value rose from 169.2 million dollars in 2021 to 316.5 in 2023 and fell to 250.5 in 2024. The BACI quantity unit is not labelled on the pages we read; we take it as tonnes because the implied values of 3 to 6 dollars a kilogram match stainless bar.
Need a quote for this part? Get a quote for your stainless parts
World flows, 2024
BACI counts about 7.0 billion dollars and 1.57 million tonnes of HS 7222 trade in 2024, down from 8.4 billion dollars in 2022. Intra-EU trade is included.
| Top exporters | Value, million dollars | Tonnes | Top importers | Value, million dollars | Tonnes |
|---|---|---|---|---|---|
| India | 1,139 | 359,000 | Germany | 948 | 215,800 |
| Italy | 1,128 | 226,000 | United States | 770 | 139,500 |
| Germany | 825 | 160,600 | Italy | 390 | 89,800 |
| United States | 528 | 44,100 | China | 358 | 48,800 |
| China | 477 | 187,300 | United Kingdom | 300 | 52,600 |
| Spain | 380 | 89,900 | France | 267 | 44,300 |
India and Italy each hold 16 percent of world export value, and India ships far more tonnes. US exports are small in tonnes but at about 12 dollars a kilogram, which marks a niche product mix.
The mirror check
Two countries reporting the same flow should be close but not equal. For 2024 we compared the EU’s exports to the US with the US’s imports from EU members:
| Source | Value | Tonnes |
|---|---|---|
| Eurostat Comext: EU27 exports to the US | 451.6 million euros | 81,159 |
| BACI: US imports from EU members | 479.3 million dollars | 79,081 |
The tonnes differ by 3 percent. The values are in different currencies, the exporter reports without freight and BACI’s reconciliation adds its own estimate, so we do not convert. Use the pair as a range and not as a single truth.
What a buyer of machined stainless parts can take from it
- Bar comes from a few countries, and the mix depends on the market. An EU buyer’s bar mostly comes from other EU members, and most of the outside supply is Indian. The largest named suppliers to the US are Italy, Germany, Taiwan and India. Ask which mill and which country each of your heats came from. See melt and pour origin on stainless bar.
- Origin now carries paperwork and a price effect. US duties sit on bar, and the EU’s 2026 steel regime may too, so ask your customs broker. Our market review and 2027 plan lists the dates, and our guide to nickel origin and forced labour checks covers what asks for more from 14 December 2027.
- A unit value is not a quote. The range from 2.52 euros a kilogram for India to 8.78 for the UK says grades and sizes differ, not that one origin is cheaper. See bar against plate cost and the stainless alloy surcharge for what moves bar price.
How to reproduce the tables
On Eurostat, open Comext dataset DS-045409, set the reporter to the EU27, the product to 7222 (or the six-digit lines), the flow to imports or exports and the indicators to value and quantity in 100 kg. Partner EXT_EU27_2020 gives the extra-EU total. For BACI, query the HS92 cube at four digits, product 7222, by exporter and importer. Check the update date on the page before you quote a number.
Next step
Use the origin tables to ask your shop a sharper question: which mill is the bar from, and in which country was it melted? Have a drawing and a destination market? Send the drawing with the grade, the bar specification and the certificate type. We send one itemised quote within 24 business hours and place the work with partner shops that cut stainless.
Sources
- Eurostat, Comext, EU trade since 1988 by HS2-4-6 and CN8 (DS-045409), HS 7222, reporter EU27, annual 2023 to 2025 and monthly to August 2026, updated 16 October 2026
- CEPII, BACI: international trade database at the product level, version 202601 of 30 January 2026, HS92, trade to 2024, queried through the Observatory of Economic Complexity on 25 October 2026
- UN Comtrade, preview API, not available during our work because the daily quota was exhausted
Figures are as read on 25 October 2026. Customs statistics are revised, so check the latest release before you quote them.
Frequently asked questions
Which HS code covers stainless steel bar?
HS 7222 covers other bars and rods of stainless steel and angles, shapes and sections of stainless steel. Hot-rolled bar in irregularly wound coils is a separate heading, 7221, and stainless wire is 7223. Machined parts fall under chapters for the finished article, so this heading describes the stock a shop buys, not the part.
Where does the EU import stainless bar from?
Mostly from other EU members. From outside the bloc, Eurostat shows 846.8 million euros and 245,018 tonnes in 2025. India supplied 481.8 million euros (57 percent), then the United Kingdom 96.5, Switzerland 78.4, the United States 72.6, Taiwan 37.2 and China 31.8.
Who sells stainless bar to the United States?
In 2024 the US imported 770.0 million dollars of HS 7222 stainless bar in the CEPII BACI database. Italy supplied 32.5 percent, Germany 12.5, Taiwan 12.3, India 11.3 and Portugal 6.9. EU members together supplied 62 percent of the value.
Do customs statistics give the price of stainless bar?
Only a unit value: customs value divided by weight. Extra-EU imports averaged 3.46 euros a kilogram in 2025, from 2.52 for India to 26.44 for US-origin bar. The figure mixes grades, sizes and finishes, so use it for direction and use quotes for price.
Need a quote for this part?
Send the drawing. We read it, send one itemised quote within 24 business hours and place the work with a partner shop that cuts stainless.
Get a quote for your stainless partsFigures in this guide are published specification limits or published typical values for the alloy, not measurements of any part. Machinability is rated against free-machining carbon steel B1112 at 100 and PREN is chromium plus 3.3 times molybdenum plus 16 times nitrogen. The conventions are set out in thereference section and the editorial standards.